Fabricante redondo de acero 4J50 de la barra Alloy50
C | Manganeso | S | Si | Ni | V | FE |
0-0.015 | 0-0.5 | 0-0.35 | 0-0.08 | balanza | 0-0.02 | 2-6 |
Nombre de producto | fabricante redondo 1Cr12 de la barra 403 1,4024 de acero |
Estándar | AISI, ASTM, estruendo, EN, SUS, UNS etc |
Técnica | Laminado en caliente en frío |
El más bajo del níquel | el ≥63% |
Material | Aleación: Aleación 20/28/31; Hastelloy: Hastelloy B/B-2/B-3/C22/C-4/S/C276/C-2000/G-35/G-30/X/N; Haynes: Haynes 230/556/188; Inconel: Inconel 100/600/601/602CA/617/625713/718738/X-750, carpintero 20; Incoloy: Incoloy 800/800H/800HT/825/925/926; GH: GH2132, GH3030, GH3039, GH3128, GH4180, GH3044 Monel: Monel 400/K500 Nitronic: Nitronic 40/50/60; Nimonic: Nimonic 75/80A/90; |
Grado | C | P | S | Manganeso | Si | Al | Ni | Co | FE |
4J42 | ≤0.05 | ≤0.02 | ≤0.02 | ≤0.8 | ≤0.3 | ≤0.1 | 41.5-42.5 | ≤1.0 | Bal. |
4J45 | ≤0.05 | ≤0.02 | ≤0.02 | ≤0.8 | ≤0.3 | ≤0.1 | 44.5-45.5 | / | Bal. |
4J50 | ≤0.05 | ≤0.02 | ≤0.02 | ≤0.8 | ≤0.3 | ≤0.1 | 49.5-50.5 | / | Bal. |
4J52 | ≤0.05 | ≤0.02 | ≤0.02 | ≤0.6 | ≤0.3 | / | 51.5-52.5 | / | Bal. |
4J54 | ≤0.05 | ≤0.02 | ≤0.02 | ≤0.6 | ≤0.3 | / | 53.5-54.5 |
Densidad (g/cm3) | 8,21 |
Resistencia eléctrica en 20ºC (ohm.mm2/m) | 0,44 |
Conductividad termal, λ/con (m*ºC) | 16,7 |
ºC del Tc/del punto del curie | 500 |
Módulo de elástico, e Gpa | 158 |
θ/ºC | α1/10-6ºC-1 | θ/ºC | α1/10-6ºC-1 |
20~100 | 9,8 | 20~400 | 9,4 |
20~200 | 9,8 | 20~450 | 9,4 |
20~300 | 9,5 | 20~500 | 9,7 |
20~350 | 9,4 | 20~600 | 10,6 |
Recocido | Calentado a 900 ±20ºC en una atmósfera del hidrógeno |
Tiempo de ocupación | 1 hora |
enfriamiento | Con velocidad no más que 5 ºC/enfriamiento mínimo debajo del ºC 200 |